規格 |
收縮率(%) |
密度(kg/m3) |
熔融指數(MVR) |
衝擊強度23℃Charpy(kJ/m2)dry/cond |
彎曲模量MPadry/cond |
HDT ℃1.8/0.45 |
性質 |
A3EG3 |
- |
1230 |
70 |
8/11 |
5000/4000 |
250/250 |
15%GF |
A3EG6 |
0.53-1.02 |
1360 |
30 |
13/22 |
8600/6500 |
250/260 |
30%GF |
A3EG6 FC |
- |
1360 |
40 |
13/22 |
8600/6500 |
250/250 |
30%GF、FDA |
A3EG7 |
0.58-1.0 |
1410 |
30 |
14/22 |
10000/8000 |
250/260 |
35%GF |
A3EG10 |
0.33-0.82 |
1560 |
8 |
18/25 |
15000/13500 |
250/260 |
50%GF |
A3HG5 |
0.48-1.06 |
1320 |
40 |
8.7/10.8 |
7600/6000 |
245/260 |
25%GF增強耐熱老化 |
A3HG6 HR |
0.45-1.15 |
1370 |
20 |
10.4/13 |
8700/5800 |
250/260 |
30%GF耐水解 |
A3HG7 |
0.37-1.04 |
1410 |
30 |
11.9/15.3 |
10000/8500 |
250/260 |
35%GF增強耐熱老化 |
A3K FC |
- |
1130 |
115 |
5/20 |
2900/- |
75/220 |
Aqua飲用水、FDA |
A3K |
1.50-1.80 |
1130 |
120 |
5/20 |
2900/- |
75/220 |
易流動、快速成型 |
A3UG5 |
0.40-1.20 |
1390 |
25 |
7.5/9 |
9500/6100 |
245/260 |
25%GF非鹵非磷V0 |
A3W |
1.50-1.80 |
1130 |
100 |
6/20 |
2900/- |
75/220 |
易流動、耐熱老化 |
A3WGM53 |
- |
1480 |
30 |
8/16 |
10100/5500 |
225/250 |
25%GF+15%M |
A3WG3 |
- |
1230 |
60 |
8/11 |
5500/4000 |
240/250 |
15%GF、耐熱老化 |
A3WG5 |
0.43-1.01 |
1320 |
40 |
12/18 |
7600/6000 |
245/250 |
25%GF、耐熱老化 |
A3WG6 |
0.38-0.93 |
1360 |
30 |
13/22 |
8600/6500 |
250/250 |
30%GF、耐熱老化 |
A3WG7 |
0.37-1.04 |
1410 |
20 |
14/22 |
10000/8000 |
250/250 |
35%GF、耐熱老化 |
A3WG10 |
0.35-0.95 |
1560 |
10 |
18/25 |
15000/13500 |
250/250 |
50%GF、耐熱老化 |
A3X2G5 |
0.39-1.04 |
1340 |
30 |
13/17 |
7100/- |
240/250 |
25%GF紅磷阻燃V0 |
A3X2G7 |
0.32-1.02 |
1450 |
25 |
14/18 |
9200/- |
240/250 |
35%GF紅磷阻燃V0 |
A3X2G10 |
- |
1600 |
25 |
13/16 |
13000/- |
250/250 |
50%GF紅磷阻燃V0 |
A3XZG5 |
- |
1320 |
- |
25/30 |
5500/- |
240/250 |
25%GF耐衝紅磷阻燃V0 |
A3Z |
- |
1060 |
21 |
90/115 |
1750/- |
60/125 |
高衝擊、耐低溫 |
A3ZG6 |
- |
1330 |
15 |
19/26 |
7300/4900 |
240/250 |
30%GF、耐衝擊 |