規格 |
收縮率% |
密度kg/m3 |
衝擊強度23℃Charpy kJ/m2 |
彎曲模量MPadry/cond |
拉伸模量MPadry/cond |
HDT℃1.8/0.45MPa |
性質 |
TC551 |
0.6-1.0 |
1520 |
- |
- |
7000/- |
- |
導熱材料、V0 |
TE250F6 |
0.4-1.1 |
1680 |
11/11 |
11000/7300 |
12000/8000 |
290/290 |
30%GF熱穩定V0 |
TE250F8 |
0.3-0.9 |
1770 |
13/14 |
13000/11000 |
15000/12000 |
290/290 |
40%GF熱穩定V0 |
TE250F9 |
0.3-0.9 |
1820 |
13/15 |
15000/11000 |
17000/12000 |
290/290 |
45%GF熱穩定V0 |
TE341 |
2.0-2.0 |
1180 |
10/35 |
3000/900 |
3300/1000 |
190/280 |
熱穩定、潤滑型 |
TE351 |
2.0-2.0 |
1370 |
8/14 |
2500/- |
3000/1200 |
160/- |
熱穩定V0 |
TS250F6D |
0.4-1.1 |
1680 |
11/11 |
11000/7300 |
12000/8000 |
290/290 |
改善回流焊接起泡 |
TS250F8 |
0.3-0.9 |
1770 |
11/12 |
13000/11000 |
15000/12000 |
290/290 |
40%GF熱穩定V0 |
TS200F6 |
0.5-1.3 |
1410 |
11/11 |
9500/5500 |
10000/6000 |
290/290 |
30%GF熱穩定V0 |
TW241F6 |
0.5-1.3 |
1410 |
12/21 |
9000/5500 |
10000/6000 |
290/290 |
30%GF熱穩定潤滑 |
TW241F8 |
0.5-1.1 |
1510 |
14/21 |
11500/7000 |
13000/8000 |
290/290 |
40%GF熱穩定潤滑 |
TW271B3 |
0.2-0.8 |
1320 |
6/- |
11000/5800 |
12500/6700 |
290/- |
15%CF摩擦磨耗改良 |
TW271B6 |
0.3-0.7 |
1320 |
7/17 |
23000/- |
24000/14500 |
290/- |
30%CF摩擦磨耗改良 |
TW271F6 |
0.5-1.3 |
1540 |
13/17 |
8500/5700 |
10000/6000 |
290/290 |
30%GF摩擦磨耗改良 |
TW271F8 |
0.6-1.1 |
1630 |
14/- |
11500/- |
13000/- |
285/285 |
40%GF摩擦磨耗改良 |
TW341-FC |
2.0-2.0 |
1180 |
10/35 |
3000/900 |
3300/1000 |
190/280 |
熱穩定、潤滑、FDA |
TW341 |
2.0-2.0 |
1180 |
10/35 |
3000/900 |
3300/1000 |
190/280 |
熱穩定、潤滑型 |
TW371 |
2.0-2.0 |
1250 |
7/15 |
2600/900 |
2900/1000 |
190/290 |
熱穩定摩擦磨耗改良 |
Stanyl® - PA46 介紹 https://www.dsm.com/markets/engineering-plastics/zh-cn/products/stanyl.html